Thermal Spray Technology



Grinding in two steps:
The first step: rough grinding, the grinding parameters are: abrasive grain size 125-150 mesh; grinding wheel RPM is 25-30m / s; workpiece RPM is 0.3m / s; grinding depth <0.01mm; moving speed 0.2-0.3 m/min, longitudinal feed amount 0.025-0.05mm
The second step:fine grinding, the grinding parameters are: abrasive grain size 380-400 mesh, grinding wheel RPM 25-30m/s; workpiece RPM 0.5m/s; grinding depth less <0.005mm, moving speed 0.05-0.1m/s, the longitudinal feed rate is 0.025-0.05mm.